Diagnose common print defects by what you can see

Practical 3D printing help, settings, projects, and advice from fellow makers.

Print troubleshooting

P0k3sm0t
Use the visible symptom to choose the first checks. Poor first-layer adhesion: clean the plate, confirm the plate type in the slicer, verify bed temperature, and inspect the first-layer offset. Stringing: dry the filament first, then verify temperature and retraction. Excessive retraction can create clogs, so use small controlled changes. Layer shifts: check belt tension, pulleys, motor cables, collisions, and acceleration. A shift at the same height can point to a model or mechanical obstruction. Under-extrusion: inspect for a partial clog, tangled spool, slipping extruder, wrong filament diameter, low temperature, or an incorrect flow setting. Warping: reduce drafts, improve plate cleanliness, use the correct bed temperature, add a brim when appropriate, and avoid unnecessary cooling on early layers. Dimensional error: calibrate motion and extrusion only with a sound method, then account for material shrinkage, hole compensation, and designed clearance. Post a clear photo and your settings if the symptom remains. Similar-looking defects can have different causes. USING THIS ON HOMEBREW PRINTING Search Slicer Studio settings for retraction, Z hop, cooling, chamber, speed, and flow. Change one variable, slice again, and save the working profile. Repair mesh addresses geometry; it does not cure a physical printer or material problem. Use forum search to find the related studio instructions for the current controls.
Sign in to reply

Edit post